Examining and repairing crankshaft
WIS 03-3180
Operation no. of operation texts and work units or standard texts and flat rates
Data iin mm
measured and one full revolution, permissible difference 0.04. 5) The limit value must exist at at least 2/3 of the circumference of the journal. 6) Related to 1st and 12th balancing weight at $50 rpm when mounted on 2nd and 6th crankshaft bearing journals.
ottign = RA 03,1225-3180/1
Note Maximum wear limit of crankshaft and conrod bearing journals 0.02 mm. The repair sizes fisted in the table should be adhered to exactly. When re-grinding, it is essential to maintain the fillet radii at the crankshaft and conrod bearing journals. All the radii of the conrod and crankshaft bearings are inductively surface-hardened, at the 2nd, 3rd, 4th, Sth and 6th crankshaft bearings. The running surface for the rear racial seal is inductively hardened to a depth of about 1–2 mm.
Special tool
Note Proceed in the order stated in the diagram overleaf when examining and servicing crankshafts.
whine = RA 03.1225-3180/2
time §=RA 03.1225-3180/3
asin = RA 03.1225-3180/4
B. Hardening
gti = RA 03,1225-3180/5
Crack testing Clean crankshaft. The bearing journals must be free of oil and grease. Magnetize crankshaft and apply fluorescent powder (flux). It is also possible to use a dye penetration method (immersing in bath or using a spray can).
Aid: — dye, UV oil or fluorescent powder, cleaning product, developer
Hardness testing Test hardness with the drop hardness tester (scleroscopic hardness). The minimum hardness of 60 scale values must exist at 2/3 of the circumference of the journal.
Hardening Always harden journals with hardened radii (arrows) inductively. If this is not possible, scrap crankshaft.
wii §=RA, 03.1225-3180/6
Corrosion protection Inspecting hardening Crankshafts which are not re-installed The setting of the hardening system should be immediately, rnust be oiled with a corrosion checked by taking metallographic sections in protection oil. order to achieve proper hardening.
These sections can be taken from test hardenings on, scrapped crankshafts.
Check hardening by etching the surface of the journal with a 2 % alcaholic nitric acid (HNO).
No dark patches should appear on the surface of the journal.
The hardened radii must be just as bright as the surface of the journal.
The non-hardened radii darken in color.
As a comparison, it is recommended to perform etching on a journal which has been metallographically checked.
Following this, carefully wash off the nitric acid with alcohol.
gigs = RA 03.1225-3180/7